ZAM™ and post hot-dip galvanized product (HDZ) show nearly the same level of corrosion potential.
Corrosion potential in different solutions (after immersion for an hour)
Corrosion potential test solutions
Solution | pH | Temperature(°C) | Remarks |
---|---|---|---|
5%NaCl | 6.5 | 35 | Solution specified in JIS Z2371 (salt spray test) |
5%NaCl+HNO3+H2SO4※1 | 3.5 | 35 | Solution specified in JIS H8502 (cyclic artificial acid rain test) |
0.1%NaCl+H2SO4※2 | 4 | 35 | Solution specified in acid rain simulated combined-cycle corrosion test |